  • 316 Stainless steel - AK Steel

    S H E E T. 316/316L-S-08-01-07. UNS S31600 AND UNS S31603. Type 316 is an austenitic chromium- nickel stainless steel containing molybdenum.

  • Stainless Steel - Grade 316 (UNS S31600) - AZoM

    13 Sep 2001 The 316 family is a group of austenitic stainless steels with superior corrosion resistance to 304 stainless steels. They also have excellent

  • Stainless Steel - Austenitic - 1.4401 Bar and Section - Aalco

    1.4401 Bar and Section. Stainless steel types 1.4401 and 1.4404 are also known as grades 316 and 316L respectively. Grade 316 is an austenitic grade second

  • 316 -316L Stainless Steel Plate - Brown McFarlane

    316-316L steels have a low Carbon content, yield and tensile strengths. Type 316 is often referred to as “marine grade” stainless due to its increased

  • Stainless steel - Wikipedia

    In metallurgy, stainless steel, also known as inox steel or inox from French inoxydable . All types of stainless steel resist attack from phosphoric acid, types 316 and 317 more so than 304; types 304L and 430 have been successfully used with

  • Stainless Steel Alloys 316/316L Datasheet | Fine Tubes

    Grade 316 is the standard molybdenum-bearing grade, second inoverall volume production to 304 amongst the austenitic stainless steels. The molybdenum

  • Stainless Steel Alloy 316/316L Specifications: UNS S31600

    Penn Stainless inventory includes 316/316L (UNS S31600 / S31603), in sheet, sheet coil, plate, plate coil, bar, structural and tubular products. Generally, this

  • 304 vs 316 Stainless Steel | Reliance Blog - Reliance Foundry Co. Ltd.

    19 Aug 2015 Stainless steel is sleek, modern, and highly resistant to rust – but some grades perform better than others. 304 and 316 are the most common

  • Stainless Steel 316 - Alloy Composition - ESPI Metals

    Stainless steel type 316 is part of a family of stainless steel alloys (301, 302, 303, 304, 316, 347). The 316 family is a group of austenitic stainless steels with

  • AISI Type 316 Stainless Steel, annealed sheet - ASM Material Data

    Subcategory: Ferrous Metal; Metal; Stainless Steel; T 300 Series Stainless Steel. Key Words: UNS S31600, SS316, 316SS, AISI 316, DIN 1.4401, DIN 1.4408,

  • 316 Stainless Steel Technical Data Sheet - MetalShims

    Types 316 and 316L are molybdenum-bearing austenitic stainless steel which are more resistant to general corrosion and pitting/crevice corrosion than the

  • 316 Stainless Steel Material Property Data Sheet - Product

    Stainless Steel 316 is stocked by 326 North American distributors and produced by 148 large mills. Distributors will offer small quantity buys while mills will

  • 316 Stainless Steel Sheet, Coil & Plate - AMS 5524, AMS 5507

    316 / 316L are asutenitic stainless steels that contain molybdenum, which increases their resistance to many chemical corrodents and marine environments.

  • 316 316L 316H - Atlas Steels

    316 316L 316H. Revised Jan 2011. Page 1 of 2 atlassteels.au. Grade 316 is the standard molybdenum-bearing austenitic grade, second stainless

  • Stainless Steel Information Knowledge | 18-8 | 304 | 316

    The differences between the different types of stainless steel are explained in a simple, easy to understand way.

  • Grade 316 Stainless Steel Technical Data

    Grade 316 Stainless Steel Physical and Mechanical Properties.

  • 316 Stainless Bar & Rod Stock - 316 SS Bars (Hex, Round & Square

    316 and 316/L (UNS S31600 & S31603) are molybdenum-bearing austenitic stainless steels that offer higher creep, stress to rupture and tensile strength at

  • 316 / 316L Stainless Steel Pipe - SS 316 & SS316L Pipe Specs | TW

    The addition of molybdenum in 316 / 316L Stainless Steel Pipe improves the alloys corrosion resistance, particularly with higher resistance to pitting and crevice

  • stainless steel - 316 / 316l - Global Metals

    notification. Global Metals takes no responsibility for any errors1 or omissions, or for any consequences resulting from its use. STAINLESS STEEL - 316 / 316L.

  • Chemical composition of stainless steel

    Chemical composition of stainless steel . SUS316, 316, Max.0.08, Max.1.00, Max.2.00, Max.0.045, Max.0.030, 10.00~14.00, 16.00~18.00, 2.00~3.00, -, -, -.